Minimum yield strength of 315 MPa and tensile range of 440–570 MPa for 32-strength higher-grade hull steel.
IACS UR W11 Rev.9 · EH32 / E32 · 315 MPa yield · −40°C Charpy
Send your EH32 plate list, thickness ranges, nominated classification society and receiving port. Get a quotation aligned with the approved producing mill, impact scope and delivery requirements.
*31 J minimum average longitudinal Charpy impact energy at −40°C for full-size specimens and plate thickness ≤50 mm; class and testing provisions apply.

Specify the E32 material strength class, full plate sizes, −40°C Charpy requirement and the producing mill approval route for your marine project.
| Steel grade | EH32 (E32 / HE32 in applicable hull steel designations) |
| Grade family | Higher-strength hull structural steel, 32 strength class, E-quality toughness |
| Technical basis | IACS UR W11 Rev.9 and the nominated classification society rules |
| Minimum yield strength | 315 MPa |
| Tensile strength | 440–570 MPa |
| Elongation | 22% minimum on the standard proportional gauge (test provisions apply) |
| Impact temperature | −40°C for EH32 / E32 |
| Reference plate thickness | IACS UR W11 general plate provisions primarily cover thickness up to 100 mm; actual mill approval governs |
| Plate size | Thickness × width × length from your schedule, confirmed against mill approval and available supply |
| Delivery condition | Normalized or thermo-mechanically rolled, with thickness and class conditions verified |
| Material documents | Heat analysis, tensile and −40°C Charpy records, heat traceability and nominated class certificate package |
| Quoted supply | EH32 grade, society, dimensions, approved producing works, inspection scope, volume and destination port |
The assigned class rules, producing mill approval range, plate thickness, delivery condition and specimen requirements govern acceptance.
Use the −40°C Charpy V-notch requirement with the appropriate plate thickness and specimen orientation in your hull steel purchase list.
| Nominal thickness | Impact temperature | Longitudinal min. avg. | Transverse min. avg. |
|---|---|---|---|
| t ≤ 50 mm | −40°C | 31 J | 22 J |
| 50 < t ≤ 70 mm | −40°C | 38 J | 26 J |
| 70 < t ≤ 100 mm | −40°C | 46 J | 31 J |
Minimum yield strength of 315 MPa and tensile range of 440–570 MPa for 32-strength higher-grade hull steel.
Specify the thickness band and longitudinal or transverse test direction with the classification requirements.
Confirm producer approval for EH32, the ordered thickness and the required class survey/material certificate.
Request the heat-specific ladle analysis and review the fine-grain practice approved for EH32 by the actual producing mill and classification society.
| Element | IACS Reference Requirement |
|---|---|
| Carbon (C) | ≤ 0.18% |
| Manganese (Mn) | 0.90–1.60%* |
| Silicon (Si) | ≤ 0.50% |
| Phosphorus (P) | ≤ 0.035% |
| Sulfur (S) | ≤ 0.035% |
| Acid-soluble aluminium (Al) | ≥ 0.015% where the Al route applies |
| Copper (Cu) | ≤ 0.35% |
| Chromium (Cr) | ≤ 0.20% |
| Nickel (Ni) | ≤ 0.40% |
| Molybdenum (Mo) | ≤ 0.08% |
The selected steelmaking practice may use aluminium, niobium, vanadium, titanium or an approved combination of grain-refining elements.
Under Table 2, the manganese minimum may decrease to 0.70% through 12.5 mm. Fine-grain element limits, supplementary chemistry and actual melt analysis are confirmed through the material certificate and class requirements.
Specify EH32 where the class-approved ship structure calls for E-quality toughness and the associated welded plate acceptance.

EH32 plate for ship hull blocks, shell plating and structural sections identified on your approved drawing.

Deck structures, longitudinal reinforcements and welded members requiring the specified EH32 toughness designation.
Grade-traceable plate for hull shell areas where E-quality impact requirements are specified.
Material for deck plates, stiffened panels and hull longitudinal elements.
Welded bulkheads and frames following the approved shipyard material list.
Fabricated support members and webs for classed hull structures.
Replacement plate purchases matched to the vessel’s class repair procedure.
Batch-traceable plate shipments grouped by hull block and work schedule.
Send the plate dimensions, −40°C Charpy scope, mill/class requirements and planned port delivery.
Identify your classification society and verify the actual producing works’ EH32 approval, thickness limits and material inspection requirements.
Verify the producing steelworks’ approval scope for E32 plate, the required thickness and rolling condition.
Check the required tensile, Charpy and heat-analysis records for EH32, including impact specimen orientation.
Match heat identification, survey records and class-related certification to the order and shipment batch.
Review hot-rolled finish, edges, dimensions and material markings against your shipyard plate acceptance list.

Surface quality, mill scale, plate identification and any protective treatment are specified in your order.

Nominal thickness, cut dimensions and inspection tolerances guide the acceptance plan.
IACS UR W11 Table 5 specifies normalized or thermo-mechanically rolled supply for E32 plates, subject to the producing mill and classification approval.
Normalized heat treatment (N) is a recognized delivery route for E32 hull plate under Table 5.
TMCP is a recognized E32 plate route when the mill process is approved and toughness criteria are met.
Through 50 mm and above 50 to 100 mm, use normalized or TMCP plate under the standard Table 5 plate route.
Specify any through-thickness testing, weld procedure or special project acceptance with the order.
| Product / practice | Nominal thickness | IACS W11 Rev.9 delivery condition |
|---|---|---|
| E32 plate / grain-refined steel | ≤50 mm | Normalized (N) or thermo-mechanically rolled (TMCP) |
| E32 plate / grain-refined steel | >50–100 mm | Normalized (N) or thermo-mechanically rolled (TMCP) |
| Sections only, special approval | According to mill/class approval | As-rolled or controlled-rolled only where the classification society specifically accepts the section route |
Coordinate E-quality hull plate sourcing, −40°C testing requirements and export shipments through one steel supply team.
Our actual annual steel production spans the company’s wider steel range and supports planned purchasing.
Your EH32 plate size list is checked against current supply and producing mill availability.
Review mill approval, normalized or TMCP condition and −40°C Charpy documents for the intended order.
Discuss plate batch identification, inspection records, shipping quantities and destination port in one enquiry.
BAOSTEEL METAL operates across steel product categories with 8 million metric tons of actual annual steel production, 500,000 m² factory area and over 1,000 employees. EH32 plate quotations depend on the actual producing mill’s approved E32 grade and thickness range.


Our regular company-wide inventory covers a broad steel product range. Send your EH32 dimensions, nominated classification society and delivery schedule to check available material and appropriate production routes.
Your order can specify material marking, chemical composition, E32 strength properties and the −40°C Charpy results required by the nominated classification society.

Estimate plate tonnage using your hull fabrication schedule and nominal steel density before submitting your RFQ.
Nominal plate density: 7,850 kg/m³. Commercial tonnage follows the agreed measurement and contract.
Identify the steel grade, thickness, nominated classification society and −40°C impact scope for each required item.
Share your shipyard plate schedule and approved project documents for review.
Include finished plate profiles, cutting drawings and edge tolerances with your EH32 material schedule.
Cutting suitability assessed against thickness and the requested plate profile.
Thermal cutting routes reviewed for the part size, plate condition and edge requirements.
Finished drilling details and prepared edges quoted with your shipyard drawings.

Provide your EH32 plate list, approved class document needs, packing preferences and destination port. Your quotation will confirm shipment grouping, loading requirements and commercial delivery terms.
Review strength class, Charpy test temperature and the nominated society’s grade requirements before changing a purchase designation.
Strength and Charpy requirements are grade-specific. Select the material required by the approved hull drawing and nominated class rules.
315 MPa minimum yield with 0°C reference Charpy testing.
View grade →315 MPa minimum yield with −20°C reference Charpy testing.
View grade →315 MPa minimum yield with −40°C reference Charpy testing.
IACS UR W11 Rev.9 defines EH32 / E32 as a 315 MPa minimum yield grade with 440–570 MPa tensile strength and 22% proportional elongation under the applicable tests.
EH32 uses −40°C Charpy testing. Full-size specimen minimum longitudinal averages are 31 J through 50 mm, 38 J above 50–70 mm and 46 J above 70–100 mm, subject to the class rules.
IACS W11 Table 5 lists normalized or TMCP supply for E32 plates within the standard thickness ranges. The approved producing mill and nominated class determine the actual order route.
Share the nominated classification society, vessel requirements, plate dimensions and survey scope. The producing mill approval, material identification, testing and required certificate package are checked for your order.
Send your EH32 plate schedule, quantity, nominated class, −40°C testing needs, delivery window, destination and any approved drawings.
Send your required grade, dimensions, quantity and destination. Our team will review the inquiry.